Show simple item record

dc.contributor.author MAZURU, Sergiu
dc.contributor.author TOCA, Alexei
dc.contributor.author TRIFAN, Nicolae
dc.contributor.author PLATON, Andrei
dc.contributor.author MAZURU, Alexandru
dc.date.accessioned 2022-09-19T07:39:28Z
dc.date.available 2022-09-19T07:39:28Z
dc.date.issued 2021
dc.identifier.citation BOSTAN, Ion, MAZURU, Sergiu, TOCA, Alexei et al. Procedeu de sulfitare a produsului vinic Procedeu de reglare a jocului axial în angrenajul conic ol. In: INFOINVENT 2021. Expoziţia Internaţională Specializată, 17-20 noiembrie 2021, ed. 17: Catalog oficial, Chişinău, Republica Moldova, 2021, p. 120. en_US
dc.identifier.uri http://repository.utm.md/handle/5014/21261
dc.description Cerere: MD a 2020 0015 din 24.02.2020. Secţiunea B. Materiale, echipamente şi tehnologii industriale, mecanică, energie, electricitate, electronică. Section B. Materials, Equipment and Industrial Technology, Mechanics, Energy, Electricity, Electronics en_US
dc.description.abstract Procedeul, include prelucrarea termică, deformarea plastică şi nitrurarea. Totodată, înainte de nitrurare produsul se încălzeşte până la temperatura de 490-540°C, cu menţinerea în atmosfera inertă timp de 20-30 min. Procesul de nitrurare se realizează ciclic, totodată fiecare ciclu este compus din două semicicluri egale după durată, iar durata fiecărui semiciclu constituie 0,5; 1; 1,5; 3 ore. La primul semiciclu procesul are loc, atunci când azotul difuzează în fier, iar la al doilea semiciclu are loc etapa de disociere a stratului nitrurat (se întrerupe alimentare cu amoniac). Semiciclurile se realizează la temperaturi diferite. en_US
dc.description.abstract The process, according to the invention, comprises heat treatment, plastic deformation and nitriding. At the same time, before nitriding, the product is heated to a temperature of 490-540°C, keeping it in an inert atmosphere for 20-3 min. The nitriding process is performed cyclically, at the same time each cycle consists of two equal in duration half-cycles, and the duration of each half-cycle is 0.5; 1; 1.5; 3 hours. In the first half-cycle, the process takes place when nitrogen diffuses into the iron, and in the second half-cycle the stage of dissociation of the nitrided layer takes place. en_US
dc.language.iso en en_US
dc.language.iso ro en_US
dc.publisher Agenţia de Stat pentru Proprietatea Intelectuală a Republicii Moldova (AGEPI) en_US
dc.rights Attribution-NonCommercial-NoDerivs 3.0 United States *
dc.rights.uri http://creativecommons.org/licenses/by-nc-nd/3.0/us/ *
dc.subject invenţii en_US
dc.subject inventions en_US
dc.subject piese din oţel en_US
dc.subject durificarea pieselor en_US
dc.subject steel parts en_US
dc.subject parts hardening en_US
dc.title Procedeu de durificare a pieselor din oţel en_US
dc.title.alternative Process for hardening of steel parts en_US
dc.type Article en_US


Files in this item

The following license files are associated with this item:

This item appears in the following Collection(s)

  • 2021
    Ediţia a XVII-a, 17 - 20 noiembrie

Show simple item record

Attribution-NonCommercial-NoDerivs 3.0 United States Except where otherwise noted, this item's license is described as Attribution-NonCommercial-NoDerivs 3.0 United States

Search DSpace


Browse

My Account